Chemical composition
Nominal: mid-range where both limits are given, the cap where only a maximum is, balance takes the remainder. Exact specified ranges below.
| Element | Name | Content % | |
|---|---|---|---|
| Main elements6 elements | |||
| Fe | Iron | Bal. | |
| Ni | Nickel | 26 – 29% | |
| Cr | Chromium | 22 – 25% | |
| Cu | Copper | 2.5 – 3.5% | |
| Mo | Molybdenum | 2.5 – 3% | |
| Ti | Titanium | 0.5 – 0.9% | |
| Element | Name | Content % | |
|---|---|---|---|
| Minor & residual5 elements | |||
| C | Carbon | ≤ 0.06% | |
| Si | Silicon | ≤ 0.8% | |
| Mn | Manganese | ≤ 0.8% | |
| S | Sulphur | ≤ 0.02% | |
| P | Phosphorus | ≤ 0.035% | |
Where this grade is recommended
Not yet in the condition-scoring matrix. Send us your service conditions and we will advise on a like-for-like basis.
Designations & equivalents
| Latin transliteration | 06KhN28MDT |
Cross-references are common near-equivalents for search and shortlisting; substitution across standards requires clause-by-clause verification. All grades in one cross-reference table →
Applicable standards
Name the standard and its edition on the order.
Frequently asked questions
What is 06ХН28МДТ (ЭИ943)?
06ХН28МДТ (ЭИ943) — Ni corrosion-resistant. Welded equipment for sulfuric acid of any concentration up to 80 °C (GOST 5632)
Which standards cover 06KhN28MDT?
GOST 5632-2014
In which forms is 06KhN28MDT available?
Tube, plate, strip, bar, forgings, wire and other forms — sizes and delivery condition confirmed per order, with EN 10204 3.1 / 3.2 certification.
Same series
Download PDF datasheet
This grade’s datasheet as an A4 PDF — for filing, printing or forwarding to colleagues.
Download PDF datasheetSupply & enquiry
For this grade we can supply, against your service conditions:
- Tube, plate, strip, bar, forgings, wire and more — with size range and lead time
- Chemistry and mechanical test report (EN 10204 3.1 / 3.2)
- Like-for-like alternatives and selection advice
- Applicable standards and inspection scope
Or email us: info@kochlin.com
Tube & pipeφ1 – 219 × 0.25 – 25 mm
Plate4.76 – 80 mm
Barφ8 – 300 mm