Chemical composition
Nominal: mid-range where both limits are given, the cap where only a maximum is, balance takes the remainder. Exact specified ranges below.
| Element | Name | Content % | |
|---|---|---|---|
| Main elements2 elements | |||
| Cu | Copper | 61 – 64% | |
| Zn | Zinc | Bal. | |
| Element | Name | Content % | |
|---|---|---|---|
| Minor & residual2 elements | |||
| Pb | Lead | ≤ 0.09% | |
| Fe | Iron | ≤ 0.05% | |
Mechanical minima by form
Guaranteed values differ by form, size and delivery condition; quotations confirm the specification, form, size and condition.
| Form | Condition | Rm MPa | Rp0.2 MPa | A ≥ % |
|---|---|---|---|---|
| Round, hexagonal, octagonal and square wire | H00 (eighth hard), ≥0.5 mm | ≥ 345 (50 ksi) | — | — |
| Round, hexagonal, octagonal and square wire | H01, 1/4 hard, ≥0.5 mm | ≥ 425 (62 ksi) | — | — |
| Round, hexagonal, octagonal and square wire | H04 (hard), ≥0.5 mm | ≥ 705 (102 ksi) | — | — |
| Round, hexagonal and octagonal wire | H08 (spring temper), ≥0.5 mm | ≥ 830 (120 ksi) | — | — |
Where this grade is recommended
Matched in 1 service conditions; ranks and scores computed from the condition-scoring matrix.
| Service condition | Industry | Temperature | Rank | Score |
|---|---|---|---|---|
| Aquaculture & harbour works | Marine & Offshore | Seawater ≤ 40 °C | 7 / 8 | 70 |
Designations & equivalents
| UNS | C27400 / C27200 |
| W.Nr. (Germany) | 2.0321 |
| EN material number (copper) | CW508L |
| EN designation | CuZn37 |
| ASTM / AISI | B134 |
| JIS (Japan) | C2700 |
| GOST (Russia) | ≈ Л63 |
Cross-references are common near-equivalents for search and shortlisting; substitution across standards requires clause-by-clause verification. All grades in one cross-reference table →
Applicable standards
6 specifications. Name the standard and its edition on the order.
Guaranteed values and required tests differ between specifications — see Mechanical minima by form for the figures per form.
Frequently asked questions
What is H62 Brass (CuZn37)?
H62 Brass (CuZn37) — Copper. General-purpose brass bar and plate
What is the maximum service temperature of H62?
Typically about 150 °C; the practical limit depends on media, stress and design life — acceptance per the governing standard.
What is the tensile strength of H62?
The specified minimum tensile strength is 345 MPa for the main product form. Minima for other forms and sizes are listed under "Mechanical minima by form" on this page.
Which standards cover H62?
ASTM B134/B134M, ASTM B36/B36M, EN 12163 (copper alloy rod), EN 12167 (copper alloy profiles and bars), EN 12449 (seamless copper tubes), EN 1652 (copper plate, sheet and strip)
Where is H62 typically used?
Aquaculture & harbour works (Marine & Offshore)
In which forms is H62 available?
Tube, plate, strip, bar, forgings, wire and other forms — sizes and delivery condition confirmed per order, with EN 10204 3.1 / 3.2 certification.
Same series
Download PDF datasheet
This grade’s datasheet as an A4 PDF — for filing, printing or forwarding to colleagues.
Download PDF datasheetSupply & enquiry
For this grade we can supply, against your service conditions:
- Tube, plate, strip, bar, forgings, wire and more — with size range and lead time
- Chemistry and mechanical test report (EN 10204 3.1 / 3.2)
- Like-for-like alternatives and selection advice
- Applicable standards and inspection scope
Or email us: info@kochlin.com
Tube & pipeφ1 – 219 × 0.25 – 25 mm
Plate4.76 – 80 mm
Barφ8 – 300 mm
Wire & filler metalsφ0.01 – 8 mm