Kochlin SPECIAL ALLOYS · SINCE 2009

Cu-OF · UNS C10200CW008A / 2.0040 · Oxygen-Free Copper (OFHC)

ГОСТ≈ М0б

Electron-tube grade high-purity copper

Copper alloysCopper
Units
Tensile Rm
235
MPa · ≥ std. min
Service limit
150
°C · indicative max
Density
8.9
g/cm³

Chemical composition

Cu+Ag 100%Minor & residual 0.05%

Nominal: mid-range where both limits are given, the cap where only a maximum is, balance takes the remainder. Exact specified ranges below.

ElementName Content %
Main elements1 element
Cu+Ag Copper (incl. silver)≥ 99.95%
ElementName Content %
Minor & residual3 elements
O Oxygen≤ 0.001%
Other Elements other than copper and silver, total (max by difference)≤ 0.05%
Deox. Metallic or other deoxidiserNot permitted

Mechanical minima by form

Guaranteed values differ by form, size and delivery condition; quotations confirm the specification, form, size and condition.

FormCondition Rm MPaRp0.2 MPaA ≥ %
Wire and filler metals
Electrolytic copper wire rod (6.4–35 mm)Hot-worked or annealed — — ≥ 30
Several forms
Sheet, strip, plate and rolled barH01, cold-rolled (1/4 hard) 235 – 290 — —
Sheet, strip, plate and rolled barH02, cold-rolled (1/2 hard) 255 – 315 — —
Sheet, strip, plate and rolled barO60, soft annealed — — —
Refinery wire bar, cake and billetGrade 2 / C10200 / OF — — —

Where this grade is recommended

Matched in 7 service conditions; ranks and scores computed from the condition-scoring matrix.

Service conditionIndustry TemperatureRankScore
Vacuum electronics Semiconductor & Vac-Electronics ≤ 400 °C 1 / 8 95
EV drive & battery busbars Automotive & Racing ≤ 120 °C 1 / 5 94
Battery tabs & collectors Hydrogen & New Energy ≤ 80 °C 1 / 4 94
Lead frames & packaging Semiconductor & Vac-Electronics ≤ 300 °C 1 / 6 92
Sputtering targets Semiconductor & Vac-Electronics Ambient 5 / 6 87
Imaging equipment & targets Medical Devices In-body (37 °C) 5 / 5 84
Coating equipment & targets Solar & Glass ≤ 600 °C 4 / 4 82

Designations & equivalents

UNSC10200
W.Nr. (Germany)2.0040
EN material number (copper)CW008A
EN designationCu-OF
Trade name(s)OFHC / OF Copper
ASTM / AISIB49 / B111 / B152 / B170 / B187 / B395
JIS (Japan)C1020
GOST (Russia)≈ М0б

Cross-references are common near-equivalents for search and shortlisting; substitution across standards requires clause-by-clause verification. All grades in one cross-reference table →

Applicable standards

8 specifications. Name the standard and its edition on the order.

Guaranteed values and required tests differ between specifications — see Mechanical minima by form for the figures per form.

Frequently asked questions

What is TU1 Oxygen-Free Copper (C10200)?

TU1 Oxygen-Free Copper (C10200) — Copper. Electron-tube grade high-purity copper

What is the maximum service temperature of TU1?

Typically about 150 °C; the practical limit depends on media, stress and design life — acceptance per the governing standard.

What is the tensile strength of TU1?

The specified minimum tensile strength is 235 MPa for the main product form. Minima for other forms and sizes are listed under "Mechanical minima by form" on this page.

Which standards cover TU1?

ASTM B49, ASTM B152/B152M, ASTM B170, ASTM B187/B187M, ASTM B111/B111M, ASTM B395/B395M, EN 12449 (seamless copper tubes), EN 1652 (copper plate, sheet and strip)

Where is TU1 typically used?

Vacuum electronics (Semiconductor & Vac-Electronics); EV drive & battery busbars (Automotive & Racing); Battery tabs & collectors (Hydrogen & New Energy); Lead frames & packaging (Semiconductor & Vac-Electronics)

In which forms is TU1 available?

Tube, plate, strip, bar, forgings, wire and other forms — sizes and delivery condition confirmed per order, with EN 10204 3.1 / 3.2 certification.

Same series

Download PDF datasheet

This grade’s datasheet as an A4 PDF — for filing, printing or forwarding to colleagues.

Download PDF datasheet

Supply & enquiry

Tube & pipeφ1 – 219 × 0.25 – 25 mmPlate4.76 – 80 mmBarφ8 – 300 mmWire & filler metalsφ0.01 – 8 mm

For this grade we can supply, against your service conditions:

Or email us: info@kochlin.com