Kochlin SPECIAL ALLOYS · SINCE 2009

ARMCO Iron

ГОСТ≈ Э / АРМКО

Solenoid cores and pole shoes — high saturation, low coercivity

Precision alloys
Units
Tensile Rm
265
MPa · ≥ std. min
Elongation A
25
% · ≥ std. min
Service limit
400
°C · indicative max
Density
7.87
g/cm³

Chemical composition

Fe 99%Minor & residual 1.2%

Nominal: elements given only as a maximum are counted at the cap; the balance takes the remainder.

ElementName Content %
Main elements1 element
Fe IronBal.
ElementName Content %
Minor & residual10 elements
C Carbon≤ 0.006%
Si Silicon≤ 0.08%
Mn Manganese≤ 0.25%
P Phosphorus≤ 0.012%
S Sulphur≤ 0.006%
Al Aluminium≤ 0.8%
Ti Titanium≤ 0.005%
Cr Chromium≤ 0.03%
Ni Nickel≤ 0.02%
Cu Copper≤ 0.02%

Magnetic properties

Guaranteed values required by the standard, by product form and size band, measured on specimens after the final magnetic anneal.

FormCondition and size bandμmax ≥Hc ≤ (A/m)ΔHc ≤ (A/m)
Magnetic test specimens from all product formsSpecimens held at 900 ± 10 °C for 1 h and cooled below 500 °C at less than 50 °C/h0.0151 H/m323.2

Minimum induction at each field strength

Field strength H, A/m20050010002500500010000
Induction B ≥, T1.231.431.531.651.741.83

The magnetic anneal is normally agreed between supplier and purchaser and varies with size; state the form, size band and the magnetic properties to be tested on the order.

Mechanical minima by form

Guaranteed values differ by form, size and delivery condition; quotations confirm the specification, form, size and condition.

FormCondition Rm MPaRp0.2 MPaA ≥ %Other requirements and notes
Plate, sheet and strip
Cold-rolled sheet and stripSupplied soft annealed — — — Also specified: Hardness 85 HV5 – 140 HV5
Other
Hot-rolled or forged bar, hot-rolled plate and stripSupplied rolled or forged; mechanical properties are an optional contract item ≥ 265 — ≥ 25 Also specified: Hardness ≤ 195 HV5

Where this grade is recommended

Matched in 2 service conditions; ranks and scores computed from the condition-scoring matrix.

Service conditionIndustry TemperatureRankScore
Motor cores & pole pieces Automotive & Racing ≤ 180 °C 3 / 4 82
Magnetic shielding & soft-magnetic parts Semiconductor & Vac-Electronics ≤ 120 °C 5 / 5 78

Designations & equivalents

Trade name(s)ARMCO iron / Vacofer S1 / Puron / Remko
GOST (Russia)≈ Э / АРМКО

Cross-references are common near-equivalents for search and shortlisting; substitution across standards requires clause-by-clause verification. All grades in one cross-reference table →

Applicable standards

Name the standard and its edition on the order.

Frequently asked questions

What is DT4C Electromagnetic Pure Iron?

DT4C Electromagnetic Pure Iron — Precision alloys. Solenoid cores and pole shoes — high saturation, low coercivity

What is the maximum service temperature of DT4C?

Typically about 400 °C; the practical limit depends on media, stress and design life — acceptance per the governing standard.

What is the tensile strength of DT4C?

The specified minimum tensile strength is 265 MPa for the main product form. Minima for other forms and sizes are listed under "Mechanical minima by form" on this page.

Which standards cover DT4C?

GB/T 6983—2022

Where is DT4C typically used?

Motor cores & pole pieces (Automotive & Racing); Magnetic shielding & soft-magnetic parts (Semiconductor & Vac-Electronics)

In which forms is DT4C available?

Tube, plate, strip, bar, forgings, wire and other forms — sizes and delivery condition confirmed per order, with EN 10204 3.1 / 3.2 certification.

Same series

Download PDF datasheet

This grade’s datasheet as an A4 PDF — for filing, printing or forwarding to colleagues.

Download PDF datasheet

Supply & enquiry

Tube & pipeφ1 – 219 × 0.25 – 25 mmPlate4.76 – 80 mmBarφ8 – 300 mmWire & filler metalsφ0.01 – 8 mm

For this grade we can supply, against your service conditions: