Kochlin SPECIAL ALLOYS · SINCE 2009
HomeGradesN09945

UNS N09945 / N09946Alloy 945 / Incoloy 945

New high-strength sour-service grade — HPHT completion tools

IncoloyNi corrosion-resistant
Units
Tensile Rm
1035
MPa · ≥ std. min
Yield Rp0.2
896
MPa · ≥ std. min
Elongation A
18
% · ≥ std. min
Service limit
540
°C · indicative max
Density
8.2
g/cm³

Chemical composition

Ni 50%Cr 21%Fe 17%Mo 3.5%Nb 3.5%Cu 2.3%Ti 1.5%Other 0.38%Minor & residual 0.50%

Nominal: mid-range where both limits are given, the cap where only a maximum is, balance takes the remainder. Exact specified ranges below.

ElementName Content %
Main elements9 elements
Ni Nickel45 – 55%
Cr Chromium19.5 – 23%
Fe IronBal.
Mo Molybdenum3 – 4%
Nb Niobium2.4 – 4.5%
Cu Copper1.5 – 3%
Ti Titanium0.5 – 2.5%
Al Aluminium0.01 – 0.7%
C Carbon0.005 – 0.04%
ElementName Content %
Minor & residual1 element
Si Silicon≤ 0.5%

Mechanical minima by form

Guaranteed values differ by form, size and delivery condition; quotations confirm the specification, form, size and condition.

FormCondition Rm MPaRp0.2 MPaA ≥ %Other requirements and notes
Seamless tube, Type 1Solution annealed, aged ≥ 1035 (150 ksi) ≥ 896 (130 ksi) ≥ 18 Also specified: Hardness ≤ 42 HRC
Seamless tube, Type 2Solution annealed, aged ≥ 1138 (165 ksi) ≥ 965 (140 ksi) ≥ 18 Also specified: Hardness ≤ 42 HRC

Where this grade is recommended

Matched in 8 service conditions; ranks and scores computed from the condition-scoring matrix.

Service conditionIndustry TemperatureRankScore
Wellhead & Christmas tree Oil & Gas ≤ 120 °C 1 / 7 93
Downhole tubing (sour H₂S/CO₂) Oil & Gas ≤ 150 °C 2 / 10 92
HPHT wells Oil & Gas 150 – 230 °C 2 / 7 92
Packers & downhole tools Oil & Gas ≤ 150 °C 3 / 7 92
Subsea lines, risers & manifolds Oil & Gas ≤ 60 °C 2 / 7 90
Valves, fittings & flanges Oil & Gas ≤ 150 °C 5 / 14 86
Drill string & non-mag collars Oil & Gas ≤ 150 °C 4 / 6 85
Platform structures & clamps Marine & Offshore Atmospheric & splash 4 / 7 85

Designations & equivalents

UNSN09945 / N09946
Trade name(s)Incoloy 945 / 945X
ASTM / AISIB983

Cross-references are common near-equivalents for search and shortlisting; substitution across standards requires clause-by-clause verification. All grades in one cross-reference table →

Applicable standards

2 specifications. Name the standard and its edition on the order.

Guaranteed values and required tests differ between specifications — see Mechanical minima by form for the figures per form.

Frequently asked questions

What is Alloy 945 · UNS N09945?

Alloy 945 · UNS N09945 — Ni corrosion-resistant. New high-strength sour-service grade — HPHT completion tools

What is the maximum service temperature of N09945?

Typically about 540 °C; the practical limit depends on media, stress and design life — acceptance per the governing standard.

What is the tensile strength of N09945?

The specified minimum tensile strength is 1035 MPa for the main product form. Minima for other forms and sizes are listed under "Mechanical minima by form" on this page.

Which standards cover N09945?

ASTM B983, AWS A5.14

Where is N09945 typically used?

Wellhead & Christmas tree (Oil & Gas); Downhole tubing (sour H₂S/CO₂) (Oil & Gas); HPHT wells (Oil & Gas); Packers & downhole tools (Oil & Gas)

In which forms is N09945 available?

Tube, plate, strip, bar, forgings, wire and other forms — sizes and delivery condition confirmed per order, with EN 10204 3.1 / 3.2 certification.

Same series

Download PDF datasheet

This grade’s datasheet as an A4 PDF — for filing, printing or forwarding to colleagues.

Download PDF datasheet

Supply & enquiry

Tube & pipeφ1 – 219 × 0.25 – 25 mmPlate4.76 – 80 mmBarφ8 – 300 mmWire & filler metalsφ0.01 – 8 mm

For this grade we can supply, against your service conditions:

Or email us: info@kochlin.com