Kochlin SPECIAL ALLOYS · SINCE 2009
HomeGradesQSn6.5-0.1

CuSn6 · UNS C51900CW452K / 2.1020 · Phosphor Bronze

ГОСТ≈ БрОФ6,5-0,15

Spring elements, bushings and washers — wear- and fatigue-resistant

Copper alloysCopper
Units
Tensile Rm
550
MPa · ≥ std. min
Service limit
200
°C · indicative max
Density
8.8
g/cm³

Chemical composition

Cu 93%Sn 6%P 0.19%Minor & residual 0.45%

Nominal: mid-range where both limits are given, the cap where only a maximum is, balance takes the remainder. Exact specified ranges below.

ElementName Content %
Main elements3 elements
Cu CopperBal.
Sn Tin5 – 7%
P Phosphorus0.03 – 0.35%
ElementName Content %
Minor & residual3 elements
Fe Iron≤ 0.1%
Pb Lead≤ 0.05%
Zn Zinc≤ 0.3%

Mechanical minima by form

Guaranteed values differ by form, size and delivery condition; quotations confirm the specification, form, size and condition.

FormCondition Rm MPaRp0.2 MPaA ≥ %
Sheet and stripO60 (soft) 330 – 435 — —
Sheet and stripH02, half hard 440 – 545 — —
Sheet and stripH04, hard 550 – 660 — —

Where this grade is recommended

Matched in 1 service conditions; ranks and scores computed from the condition-scoring matrix.

Service conditionIndustry TemperatureRankScore
Lightweight parts & springs Automotive & Racing 150 – 300 °C 3 / 7 78

Designations & equivalents

UNSC51900
W.Nr. (Germany)2.1020
EN material number (copper)CW452K
EN designationCuSn6
Trade name(s)Phosphor Bronze
ASTM / AISIB103
JIS (Japan)C5191
GOST (Russia)≈ БрОФ6,5-0,15

Cross-references are common near-equivalents for search and shortlisting; substitution across standards requires clause-by-clause verification. All grades in one cross-reference table →

Applicable standards

5 specifications. Name the standard and its edition on the order.

Guaranteed values and required tests differ between specifications — see Mechanical minima by form for the figures per form.

Frequently asked questions

What is Phosphor Bronze QSn6.5-0.1?

Phosphor Bronze QSn6.5-0.1 — Copper. Spring elements, bushings and washers — wear- and fatigue-resistant

What is the maximum service temperature of QSn6.5-0.1?

Typically about 200 °C; the practical limit depends on media, stress and design life — acceptance per the governing standard.

What is the tensile strength of QSn6.5-0.1?

The specified minimum tensile strength is 550 MPa for the main product form. Minima for other forms and sizes are listed under "Mechanical minima by form" on this page.

Which standards cover QSn6.5-0.1?

ASTM B103/B103M, EN 12163 (copper alloy rod), EN 12167 (copper alloy profiles and bars), EN 12449 (seamless copper tubes), EN 1652 (copper plate, sheet and strip)

Where is QSn6.5-0.1 typically used?

Lightweight parts & springs (Automotive & Racing)

In which forms is QSn6.5-0.1 available?

Tube, plate, strip, bar, forgings, wire and other forms — sizes and delivery condition confirmed per order, with EN 10204 3.1 / 3.2 certification.

Same series

Download PDF datasheet

This grade’s datasheet as an A4 PDF — for filing, printing or forwarding to colleagues.

Download PDF datasheet

Supply & enquiry

Tube & pipeφ1 – 219 × 0.25 – 25 mmPlate4.76 – 80 mmBarφ8 – 300 mmWire & filler metalsφ0.01 – 8 mm

For this grade we can supply, against your service conditions:

Or email us: info@kochlin.com