Supply range

| Size | To the order drawing |
|---|---|
| Condition | Solution-annealed or annealed; rough- or finish-machined |
| Testing | Mechanical test report; ultrasonic testing as ordered |
Sizes and conditions outside the standards can be supplied by agreement; please confirm on enquiry.
Types

For flanges, seal rings and vessel nozzles.

For tubesheets, valve bodies and blinds.

For pump and agitator shafts and large-diameter bar.
Standards and size range
| Standard | Covers | Size range |
|---|---|---|
| ASTM B564 | Nickel-alloy forgings | Dimensions and tolerances entirely to the order drawing; the standard sets none |
| ASTM B462 | Nickel-alloy forged flanges, fittings and valve parts for corrosive service | per standard |
| ASTM B381 | Titanium forgings | Mechanical properties guaranteed up to 1 935 mm² section; larger sections by agreement |
| ASTM A182 | Duplex and super-austenitic stainless forgings | Flanges, elbows and tees may not be machined directly from bar |
| Drawing | All forgings are made to drawing | |
These are the limits set by each standard, not our supply range; larger sizes can be supplied by agreement, with mechanical properties agreed separately.
Manufacturing and inspection
- Forged from qualified ingot or billet, then solution-annealed or annealed to the material specification.
- Tensile specimens are taken at mid-radius (mid-wall for hollow forgings), parallel to the direction of metal flow.
- Every lot is checked by PMI to confirm the alloy.
- EN 10204 3.1 certificates with every delivery; 3.2 with third-party witnessing on request.
Need a quote?
Send your specification, drawing or material list as it is; a grade and size are enough to start, and we confirm the rest in our reply. · info@kochlin.com
Other products
Tube & pipeSeamless and welded; heat-exchanger, instrument and U-bend tubePlateHot- and cold-rolled; sheared, waterjet-cut or cut to drawingStripCold-rolled strip and sheet; slit, 8K finish availableBarRound, square, hexagon and flat; turned or groundWire & filler metalsFine, spring and heating wire; nickel and titanium filler wirePipe fittings & flangesFlanges, elbows, tees, reducers, caps and stub ends