Kochlin SPECIAL ALLOYS · SINCE 2009

LC-Ni99 · UNS N022012.4068 · Nickel 201

ГОСТ≈ НП1

Low-carbon grade — preferred above 315 °C and for welded structures

Pure nickelNi corrosion-resistant
Units
Tensile Rm
345
MPa · ≥ std. min
Yield Rp0.2
70
MPa · ≥ std. min
Elongation A
40
% · ≥ std. min
Service limit
320
°C · indicative max
Density
8.9
g/cm³

Chemical composition

Ni 99%Minor & residual 1.4%

Nominal: mid-range where both limits are given, the cap where only a maximum is, balance takes the remainder. Exact specified ranges below.

ElementName Content %
Main elements1 element
Ni Nickel (incl. cobalt, by difference)≥ 99%
ElementName Content %
Minor & residual6 elements
Cu Copper≤ 0.25%
Fe Iron≤ 0.4%
Mn Manganese≤ 0.35%
C Carbon≤ 0.02%
Si Silicon≤ 0.35%
S Sulphur≤ 0.01%

Mechanical minima by form

Guaranteed values differ by form, size and delivery condition; quotations confirm the specification, form, size and condition.

FormCondition Rm MPaRp0.2 MPaA ≥ %
Bar and forgings
Bar and rodAnnealed, all sizes ≥ 345 (50 ksi) ≥ 70 (10 ksi) ≥ 40
Bar and rodHot-worked, all sizes ≥ 345 (50 ksi) ≥ 70 (10 ksi) ≥ 40
Tube and pipe
Welded pipe and tube (OD ≤127 mm)Annealed ≥ 345 (50 ksi) ≥ 80 (12 ksi) ≥ 35
Welded pipe and tube (OD >127 mm)Annealed ≥ 345 (50 ksi) ≥ 70 (10 ksi) ≥ 40
Welded pipe and tube (all sizes)Stress-relieved ≥ 415 (60 ksi) ≥ 205 (30 ksi) ≥ 15

Where this grade is recommended

Matched in 5 service conditions; ranks and scores computed from the condition-scoring matrix.

Service conditionIndustry TemperatureRankScore
Caustic & molten alkali Chemical Processing ≤ 80 °C 2 / 5 92
Water electrolysis Hydrogen & New Energy ≤ 90 °C 3 / 5 90
High-purity media Pharma & Fine Chemicals ≤ 80 °C 3 / 5 88
Hydrofluoric acid Chemical Processing ≤ 50 °C 5 / 6 86
Vacuum electronics Semiconductor & Vac-Electronics ≤ 400 °C 6 / 8 85

Designations & equivalents

UNSN02201
W.Nr. (Germany)2.4068
EN designationLC-Ni99
Trade name(s)Nickel 201
ASTM / AISIB160 / B161 / B162 / B163 / B366 / B725 / B730
AMS (SAE aerospace)5553
GOST (Russia)≈ НП1

Cross-references are common near-equivalents for search and shortlisting; substitution across standards requires clause-by-clause verification. All grades in one cross-reference table →

Applicable standards

7 specifications. Name the standard and its edition on the order.

Guaranteed values and required tests differ between specifications — see Mechanical minima by form for the figures per form.

Frequently asked questions

What is Nickel 201 (low-carbon)?

Nickel 201 (low-carbon) — Ni corrosion-resistant. Low-carbon grade — preferred above 315 °C and for welded structures

What is the maximum service temperature of N4?

Typically about 320 °C; the practical limit depends on media, stress and design life — acceptance per the governing standard.

What is the tensile strength of N4?

The specified minimum tensile strength is 345 MPa for the main product form. Minima for other forms and sizes are listed under "Mechanical minima by form" on this page.

Which standards cover N4?

ASTM B160, ASTM B161, ASTM B162, ASTM B163, ASTM B725, ASTM B730, AMS 5553

Where is N4 typically used?

Caustic & molten alkali (Chemical Processing); Water electrolysis (Hydrogen & New Energy); High-purity media (Pharma & Fine Chemicals); Hydrofluoric acid (Chemical Processing)

In which forms is N4 available?

Tube, plate, strip, bar, forgings, wire and other forms — sizes and delivery condition confirmed per order, with EN 10204 3.1 / 3.2 certification.

Same series

Download PDF datasheet

This grade’s datasheet as an A4 PDF — for filing, printing or forwarding to colleagues.

Download PDF datasheet

Supply & enquiry

Tube & pipeφ1 – 219 × 0.25 – 25 mmPlate4.76 – 80 mmBarφ8 – 300 mmWire & filler metalsφ0.01 – 8 mm

For this grade we can supply, against your service conditions:

Or email us: info@kochlin.com