Chemical composition
Nominal: mid-range where both limits are given, the cap where only a maximum is, balance takes the remainder. Exact specified ranges below.
| Element | Name | Content % | |
|---|---|---|---|
| Main elements1 element | |||
| Ni | Nickel (incl. cobalt, by difference) | ≥ 99% | |
| Element | Name | Content % | |
|---|---|---|---|
| Minor & residual6 elements | |||
| Cu | Copper | ≤ 0.25% | |
| Fe | Iron | ≤ 0.4% | |
| Mn | Manganese | ≤ 0.35% | |
| C | Carbon | ≤ 0.15% | |
| Si | Silicon | ≤ 0.35% | |
| S | Sulphur | ≤ 0.01% | |
Mechanical minima by form
Guaranteed values differ by form, size and delivery condition; quotations confirm the specification, form, size and condition.
| Form | Condition | Rm MPa | Rp0.2 MPa | A ≥ % |
|---|---|---|---|---|
| Bar and rod | Annealed, all sizes | ≥ 380 (55 ksi) | ≥ 105 (15 ksi) | ≥ 40 |
| Bar and rod | Hot-worked, all sizes | ≥ 415 (60 ksi) | ≥ 105 (15 ksi) | ≥ 35 |
| Cold-worked round bar (≤25.4 mm) | As-worked | ≥ 550 (80 ksi) | ≥ 415 (60 ksi) | ≥ 10 |
| Cold-worked round bar (>25.4–101.6 mm) | As-worked | ≥ 515 (75 ksi) | ≥ 345 (50 ksi) | ≥ 15 |
| Forgings, flanges and fitting stock | Annealed | ≥ 380 (55 ksi) | ≥ 105 (15 ksi) | ≥ 40 |
Where this grade is recommended
Matched in 9 service conditions; ranks and scores computed from the condition-scoring matrix.
| Service condition | Industry | Temperature | Rank | Score |
|---|---|---|---|---|
| Caustic & molten alkali | Chemical Processing | ≤ 80 °C | 1 / 5 | 94 |
| Water electrolysis | Hydrogen & New Energy | ≤ 90 °C | 1 / 5 | 92 |
| High-purity media | Pharma & Fine Chemicals | ≤ 80 °C | 1 / 5 | 90 |
| Hydrofluoric acid | Chemical Processing | ≤ 50 °C | 3 / 6 | 88 |
| Specialty gas lines | Semiconductor & Vac-Electronics | ≤ 120 °C | 3 / 4 | 88 |
| Battery tabs & collectors | Hydrogen & New Energy | ≤ 80 °C | 3 / 4 | 86 |
| Lyophilisation & cryo | Pharma & Fine Chemicals | −80 ~ 20 °C | 3 / 4 | 84 |
| Sterile reactors & piping | Pharma & Fine Chemicals | ≤ 150 °C | 5 / 5 | 84 |
| CIP / SIP systems | Pharma & Fine Chemicals | 80 – 134 °C | 4 / 4 | 82 |
Designations & equivalents
| UNS | N02200 |
| W.Nr. (Germany) | 2.4066 |
| EN designation | Ni99.2 |
| Trade name(s) | Nickel 200 |
| ASTM / AISI | B160 / B161 / B162 / B163 / B366 / B564 / B725 / B730 |
| GOST (Russia) | ≈ НП2 |
Cross-references are common near-equivalents for search and shortlisting; substitution across standards requires clause-by-clause verification. All grades in one cross-reference table →
Applicable standards
7 specifications. Name the standard and its edition on the order.
Guaranteed values and required tests differ between specifications — see Mechanical minima by form for the figures per form.
Frequently asked questions
What is Nickel 200?
Nickel 200 — Ni corrosion-resistant. Commercially pure nickel — standard for hot caustic and hydrofluoric acid
What is the maximum service temperature of N6?
Typically about 320 °C; the practical limit depends on media, stress and design life — acceptance per the governing standard.
What is the tensile strength of N6?
The specified minimum tensile strength is 380 MPa for the main product form. Minima for other forms and sizes are listed under "Mechanical minima by form" on this page.
Which standards cover N6?
ASTM B160, ASTM B161, ASTM B162, ASTM B163, ASTM B564 (forgings), ASTM B725, ASTM B730
Where is N6 typically used?
Caustic & molten alkali (Chemical Processing); Water electrolysis (Hydrogen & New Energy); High-purity media (Pharma & Fine Chemicals); Hydrofluoric acid (Chemical Processing)
In which forms is N6 available?
Tube, plate, strip, bar, forgings, wire and other forms — sizes and delivery condition confirmed per order, with EN 10204 3.1 / 3.2 certification.
Same series
Download PDF datasheet
This grade’s datasheet as an A4 PDF — for filing, printing or forwarding to colleagues.
Download PDF datasheetSupply & enquiry
For this grade we can supply, against your service conditions:
- Tube, plate, strip, bar, forgings, wire and more — with size range and lead time
- Chemistry and mechanical test report (EN 10204 3.1 / 3.2)
- Like-for-like alternatives and selection advice
- Applicable standards and inspection scope
Or email us: info@kochlin.com
Tube & pipeφ1 – 219 × 0.25 – 25 mm
Plate4.76 – 80 mm
Barφ8 – 300 mm
Wire & filler metalsφ0.01 – 8 mm