Kochlin SPECIAL ALLOYS · SINCE 2009

Cu-ETP · UNS C11000CW004A / 2.0060 · ETP Copper

ГОСТ≈ М1

Conductive/thermal base metal — power and heat transfer

Copper alloysCopper
Units
Tensile Rm
235
MPa · ≥ std. min
Service limit
150
°C · indicative max
Density
8.9
g/cm³

Chemical composition

Cu+Ag 100%Minor & residual 0.32%

Nominal: mid-range where both limits are given, the cap where only a maximum is, balance takes the remainder. Exact specified ranges below.

ElementName Content %
Main elements1 element
Cu+Ag Copper (incl. silver)≥ 99.9%
ElementName Content %
Minor & residual3 elements
Other Elements other than copper and silver, total (max by difference)≤ 0.1%
Other Any single element other than copper and silver (implied by the total)≤ 0.1%
Ag Optional silver addition (max by agreement)≤ 0.12%

Mechanical minima by form

Guaranteed values differ by form, size and delivery condition; quotations confirm the specification, form, size and condition.

FormCondition Rm MPaRp0.2 MPaA ≥ %
Bar and forgings
Bus bar, round bar and rodO60, soft annealed 195 – 255 ≥ 55 (8 ksi) ≥ 25
Wire and filler metals
Electrolytic copper wire rod (6.4–35 mm)Hot-worked or annealed — — ≥ 30
Several forms
Sheet, strip, plate and rolled barH01, cold-rolled (1/4 hard) 235 – 290 — —
Sheet, strip, plate and rolled barH02, cold-rolled (1/2 hard) 255 – 315 — —
Sheet, strip, plate and rolled barO60, soft annealed — — —

Where this grade is recommended

Matched in 4 service conditions; ranks and scores computed from the condition-scoring matrix.

Service conditionIndustry TemperatureRankScore
EV drive & battery busbars Automotive & Racing ≤ 120 °C 2 / 5 92
Battery tabs & collectors Hydrogen & New Energy ≤ 80 °C 2 / 4 92
Lead frames & packaging Semiconductor & Vac-Electronics ≤ 300 °C 4 / 6 88
PV mounting & frames Solar & Glass Ambient outdoor 2 / 3 80

Designations & equivalents

UNSC11000
W.Nr. (Germany)2.0060
EN material number (copper)CW004A
EN designationCu-ETP
Trade name(s)ETP Copper / Cu-ETP
ASTM / AISIB49 / B152 / B187 / B283
JIS (Japan)C1100
GOST (Russia)≈ М1

Cross-references are common near-equivalents for search and shortlisting; substitution across standards requires clause-by-clause verification. All grades in one cross-reference table →

Applicable standards

6 specifications. Name the standard and its edition on the order.

Guaranteed values and required tests differ between specifications — see Mechanical minima by form for the figures per form.

Frequently asked questions

What is T2 Copper (C11000 ETP)?

T2 Copper (C11000 ETP) — Copper. Conductive/thermal base metal — power and heat transfer

What is the maximum service temperature of T2?

Typically about 150 °C; the practical limit depends on media, stress and design life — acceptance per the governing standard.

What is the tensile strength of T2?

The specified minimum tensile strength is 235 MPa for the main product form. Minima for other forms and sizes are listed under "Mechanical minima by form" on this page.

Which standards cover T2?

ASTM B49, ASTM B152/B152M, ASTM B187/B187M, ASTM B283/B283M, EN 12449 (seamless copper tubes), EN 1652 (copper plate, sheet and strip)

Where is T2 typically used?

EV drive & battery busbars (Automotive & Racing); Battery tabs & collectors (Hydrogen & New Energy); Lead frames & packaging (Semiconductor & Vac-Electronics); PV mounting & frames (Solar & Glass)

In which forms is T2 available?

Tube, plate, strip, bar, forgings, wire and other forms — sizes and delivery condition confirmed per order, with EN 10204 3.1 / 3.2 certification.

Same series

Download PDF datasheet

This grade’s datasheet as an A4 PDF — for filing, printing or forwarding to colleagues.

Download PDF datasheet

Supply & enquiry

Tube & pipeφ1 – 219 × 0.25 – 25 mmPlate4.76 – 80 mmBarφ8 – 300 mmWire & filler metalsφ0.01 – 8 mm

For this grade we can supply, against your service conditions: