Heat-resistant Ni-Cr-Al alloy: hot-gas line parts and equipment, long-term service to 1200 °C; also for resistance heating elements (GOST 5632)

GOST alloysNi superalloys
Units

Chemical composition

Ni 56%Fe 23%Cr 17%Al 3%Minor & residual 1.4%

Nominal: mid-range where both limits are given, the cap where only a maximum is, balance takes the remainder. Exact specified ranges below.

ElementName Content %
Main elements4 elements
Ni Nickel55 – 58%
Fe IronBal.
Cr Chromium15 – 18%
Al Aluminium2.6 – 3.5%
ElementName Content %
Minor & residual7 elements
C Carbon≤ 0.1%
Si Silicon≤ 0.8%
Mn Manganese≤ 0.3%
S Sulphur≤ 0.02%
P Phosphorus≤ 0.02%
Ba Barium≤ 0.1%
Ce Cerium≤ 0.03%

Where this grade is recommended

Not yet in the condition-scoring matrix. Send us your service conditions and we will advise on a like-for-like basis.

Designations & equivalents

Latin transliterationKhN60Yu

Cross-references are common near-equivalents for search and shortlisting; substitution across standards requires clause-by-clause verification. All grades in one cross-reference table →

Applicable standards

Name the standard and its edition on the order.

Frequently asked questions

What is ХН60Ю (ЭИ559А)?

ХН60Ю (ЭИ559А) — Ni superalloys. Heat-resistant Ni-Cr-Al alloy: hot-gas line parts and equipment, long-term service to 1200 °C; also for resistance heating elements (GOST 5632)

Which standards cover KhN60Yu?

GOST 5632-2014

In which forms is KhN60Yu available?

Tube, plate, strip, bar, forgings, wire and other forms — sizes and delivery condition confirmed per order, with EN 10204 3.1 / 3.2 certification.

Same series

Download PDF datasheet

This grade’s datasheet as an A4 PDF — for filing, printing or forwarding to colleagues.

Download PDF datasheet

Supply & enquiry

Tube & pipeφ1 – 219 × 0.25 – 25 mmPlate4.76 – 80 mmBarφ8 – 300 mmWire & filler metalsφ0.01 – 8 mm

For this grade we can supply, against your service conditions:

Or email us: info@kochlin.com