06KhN28MT06ХН28МТ (ЭИ628)

Welded structures in less aggressive media: sulfuric acid up to 20 % at no more than 60 °C, hot phosphoric acid (GOST 5632)

GOST alloysNi corrosion-resistant
Units

Chemical composition

Fe 45%Ni 27%Cr 23%Mo 2.1%Ti 0.55%Minor & residual 1.7%

Nominal: mid-range where both limits are given, the cap where only a maximum is, balance takes the remainder. Exact specified ranges below.

ElementName Content %
Main elements5 elements
Fe IronBal.
Ni Nickel26 – 29%
Cr Chromium22 – 25%
Mo Molybdenum1.8 – 2.5%
Ti Titanium0.4 – 0.7%
ElementName Content %
Minor & residual5 elements
C Carbon≤ 0.06%
Si Silicon≤ 0.8%
Mn Manganese≤ 0.8%
S Sulphur≤ 0.02%
P Phosphorus≤ 0.035%

Where this grade is recommended

Not yet in the condition-scoring matrix. Send us your service conditions and we will advise on a like-for-like basis.

Designations & equivalents

Latin transliteration06KhN28MT

Cross-references are common near-equivalents for search and shortlisting; substitution across standards requires clause-by-clause verification. All grades in one cross-reference table →

Applicable standards

Name the standard and its edition on the order.

Frequently asked questions

What is 06ХН28МТ (ЭИ628)?

06ХН28МТ (ЭИ628) — Ni corrosion-resistant. Welded structures in less aggressive media: sulfuric acid up to 20 % at no more than 60 °C, hot phosphoric acid (GOST 5632)

Which standards cover 06KhN28MT?

GOST 5632-2014

In which forms is 06KhN28MT available?

Tube, plate, strip, bar, forgings, wire and other forms — sizes and delivery condition confirmed per order, with EN 10204 3.1 / 3.2 certification.

Same series

Download PDF datasheet

This grade’s datasheet as an A4 PDF — for filing, printing or forwarding to colleagues.

Download PDF datasheet

Supply & enquiry

Tube & pipeφ1 – 219 × 0.25 – 25 mmPlate4.76 – 80 mmBarφ8 – 300 mmWire & filler metalsφ0.01 – 8 mm

For this grade we can supply, against your service conditions: