Chemical composition
Nominal: mid-range where both limits are given, the cap where only a maximum is, balance takes the remainder. Exact specified ranges below.
| Element | Name | Content % | |
|---|---|---|---|
| Main elements8 elements | |||
| Ni | Nickel | Bal. | |
| Cr | Chromium | 28 – 31.5% | |
| Fe | Iron | 13 – 17% | |
| Mo | Molybdenum | 4 – 6% | |
| Co | Cobalt | ≤ 5% | |
| W | Tungsten | 1.5 – 4% | |
| Cu | Copper | 1 – 2.4% | |
| Nb | Niobium | 0.3 – 1.5% | |
| Element | Name | Content % | |
|---|---|---|---|
| Minor & residual4 elements | |||
| C | Carbon | ≤ 0.03% | |
| Mn | Manganese | ≤ 1.5% | |
| Si | Silicon | ≤ 0.8% | |
| S | Sulphur | ≤ 0.02% | |
Mechanical minima by form
Guaranteed values differ by form, size and delivery condition; quotations confirm the specification, form, size and condition.
| Form | Condition | Rm MPa | Rp0.2 MPa | A ≥ % | Other requirements and notes |
|---|---|---|---|---|---|
| Bar and forgings | |||||
| Bar | Annealed, dia. 7.94-88.9 mm | ≥ 586 (85 ksi) | ≥ 241 (35 ksi) | ≥ 30 | |
| Forgings, flanges, fittings and valve parts | Solution annealed | ≥ 586 (85 ksi) | ≥ 241 (35 ksi) | ≥ 30 | |
| Plate, sheet and strip | |||||
| Plate, sheet and strip | Annealed; plate 4.76–63.5 mm, sheet and strip over 0.51 mm | ≥ 586 (85 ksi) | ≥ 241 (35 ksi) | ≥ 30 | |
| Tube and pipe | |||||
| Seamless pipe and tube | Solution annealed and descaled | ≥ 586 (85 ksi) | ≥ 241 (35 ksi) | ≥ 30 | |
| Automatic fusion-welded pipe | Class I: solution annealed after welding; Class II: cold worked after welding, then solution annealed | ≥ 586 (85 ksi) | ≥ 241 (35 ksi) | ≥ 30 | |
| Fittings and flanges | |||||
| Formed fittings | Final heat-treated condition; recommended set temperature not less than 1177 °C, then rapidly air or water cooled | — | — | — | |
| Fittings (factory-made wrought butt-weld / socket) | 2150 °F [1177 °C] minimum, rapid air or water quench | — | — | — | Tensile properties follow the starting material. No tension test on the finished fitting unless agreed. Minimum temperature. |
Where this grade is recommended
Matched in 2 service conditions; ranks and scores computed from the condition-scoring matrix.
| Service condition | Industry | Temperature | Rank | Score |
|---|---|---|---|---|
| Phosphoric acid | Chemical Processing | ≤ 80 °C | 1 / 7 | 92 |
| Sulphuric acid | Chemical Processing | ≤ 80 °C | 6 / 8 | 85 |
Designations & equivalents
| UNS | N06030 / W86030 (weld) |
| W.Nr. (Germany) | 2.4603 |
| EN designation | NiCr30FeMo |
| Trade name(s) | Hastelloy G-30 / Nicrofer 4823 hMo |
| ASTM / AISI | B366 / B462 / B472 / B581 / B582 / B619 / B622 |
| NACE sour service | ISO 15156-3: annealed, no limit on H₂S or temperature; cold-worked ≤40 HRC |
Cross-references are common near-equivalents for search and shortlisting; substitution across standards requires clause-by-clause verification. All grades in one cross-reference table →
Applicable standards
7 specifications. Name the standard and its edition on the order.
Guaranteed values and required tests differ between specifications — see Mechanical minima by form for the figures per form.
Frequently asked questions
What is Alloy G-30 · UNS N06030?
Alloy G-30 · UNS N06030 — Ni corrosion-resistant. Phosphoric acid, mixed acids and slurry environments
What is the maximum service temperature of N06030?
Typically about 480 °C; the practical limit depends on media, stress and design life — acceptance per the governing standard.
What is the tensile strength of N06030?
The specified minimum tensile strength is 586 MPa for the main product form. Minima for other forms and sizes are listed under "Mechanical minima by form" on this page.
Which standards cover N06030?
ASTM B582, ASTM B581, ASTM B622, ASTM B619/B619M, ASTM B462, ASTM B472, ASTM B366/B366M
Where is N06030 typically used?
Phosphoric acid (Chemical Processing); Sulphuric acid (Chemical Processing)
In which forms is N06030 available?
Tube, plate, strip, bar, forgings, wire and other forms — sizes and delivery condition confirmed per order, with EN 10204 3.1 / 3.2 certification.
Same series
Download PDF datasheet
This grade’s datasheet as an A4 PDF — for filing, printing or forwarding to colleagues.
Download PDF datasheetSupply & enquiry
For this grade we can supply, against your service conditions:
- Tube, plate, strip, bar, forgings, wire and more — with size range and lead time
- Chemistry and mechanical test report (EN 10204 3.1 / 3.2)
- Like-for-like alternatives and selection advice
- Applicable standards and inspection scope
Or email us: info@kochlin.com
Tube & pipeφ1 – 219 × 0.25 – 25 mm
Plate4.76 – 80 mm
Barφ8 – 300 mm
Wire & filler metalsφ0.01 – 8 mm