ГОСТ≈ 49К2Ф

Highest saturation induction (2.4 T) — electromagnet pole pieces and high-power-density motors

Precision alloys
Units
Service limit
500
°C · indicative max
Density
8.12
g/cm³

Physical properties

Density8.12g/cm³

Informative values: they vary with composition, condition and test method. Use the governing standard or measured mill data for pressure and heat-transfer calculations.

Chemical composition

Fe 49%Co 49%V 1.9%Minor & residual 0.75%

Nominal: mid-range where both limits are given, the cap where only a maximum is, balance takes the remainder. Exact specified ranges below.

ElementName Content %
Main elements3 elements
Fe IronBal.
Co Cobalt47.5 – 49.5%
V Vanadium1.75 – 2.1%
ElementName Content %
Minor & residual7 elements
C Carbon≤ 0.025%
Mn Manganese≤ 0.15%
Si Silicon≤ 0.15%
P Phosphorus≤ 0.015%
S Sulphur≤ 0.01%
Cr Chromium≤ 0.15%
Ni Nickel≤ 0.25%

Mechanical minima by form

Guaranteed values differ by form, size and delivery condition; quotations confirm the specification, form, size and condition.

FormCondition Rm MPaRp0.2 MPaA ≥ %
Plate, sheet and strip
Cold-rolled stripMagnetic heat treatment to an agreed procedure — — —
Several forms
Bar, forging stock and hot-rolled sheet and stripMagnetic heat treatment to an agreed procedure — — —

Where this grade is recommended

Matched in 2 service conditions; ranks and scores computed from the condition-scoring matrix.

Service conditionIndustry TemperatureRankScore
Motor cores & pole pieces Automotive & Racing ≤ 180 °C 1 / 4 93
Magnetic shielding & soft-magnetic parts Semiconductor & Vac-Electronics ≤ 120 °C 4 / 5 80

Designations & equivalents

Trade name(s)Hiperco 50 / Permendur / Vacoflux 50 / Supermendur / 2V-Permendur
GOST (Russia)≈ 49К2Ф

Cross-references are common near-equivalents for search and shortlisting; substitution across standards requires clause-by-clause verification. All grades in one cross-reference table →

Applicable standards

Name the standard and its edition on the order.

Frequently asked questions

What is 1J22 Fe-Co-V Soft Magnetic (Hiperco 50 class)?

1J22 Fe-Co-V Soft Magnetic (Hiperco 50 class) — Precision alloys. Highest saturation induction (2.4 T) — electromagnet pole pieces and high-power-density motors

What is the maximum service temperature of 1J22?

Typically about 500 °C; the practical limit depends on media, stress and design life — acceptance per the governing standard.

Which standards cover 1J22?

ASTM A801

Where is 1J22 typically used?

Motor cores & pole pieces (Automotive & Racing); Magnetic shielding & soft-magnetic parts (Semiconductor & Vac-Electronics)

In which forms is 1J22 available?

Tube, plate, strip, bar, forgings, wire and other forms — sizes and delivery condition confirmed per order, with EN 10204 3.1 / 3.2 certification.

Same series

Download PDF datasheet

This grade’s datasheet as an A4 PDF — for filing, printing or forwarding to colleagues.

Download PDF datasheet